Flux Frequently Asked Questions and Answers 2 Empty welding
Printing: bias,
Path: bias, mounting pressure, poor thimble positioning
Reflow welding: the temperature setting is not good, the component is not heated enough.
Materials:1. Poor weldability of components. 2. The activity of solder p